innovate wrote:What is the temp on your extruder?
Its between 193 196 degrees celcius steady
ronsii wrote:Since it is black you will probably have to bump the temp up a few degrees. Can't tell you much other then that without more details...
Never knew that, Why is that? Anyway I tried with other colors and the same happens.
3d-oodler wrote:Also, how much temp variations do you see?
Its between 193 196 degrees celcius steady
3d-oodler wrote:Have you PID autotuned?
I did a google search and i think this is to make the temperature stable but it already is so I don't think this is
3d-oodler wrote:Have you calibrated your extruder steps?
I don't think this will help because the printer runs normally for a few layers and then a few layers of ugly