frozensoda wrote:Mr.Factotum wrote:Any Suggestions on getting the prints to stick well to the kapton? I am Using Octave White with 195C on the extruder and 95C on the bed. The bed is level and the Z offset is just right, But about a quarter the way into a print one corner will begin to peel up and I kill the print. Any Suggestions?
a light coating of hairspray, and setting the brim to 4mm, and setting first layer speed to 60%
After I did these things I never had another warped print. The hairspray lasts for a long time and you really only need to clean it off when it becomes too thick to be level.
+1 on all this. I run my 1st layer speed at 50% On large prints that are a 100mm or more, I set my 1st layer extrusion width to 200% and run a 6mm brim. On prints between 50mm-100mm i'll use a brim of 4mm. Anything less than that, 1st layer width to 150% and no brim.
I'm using the stock SD3 bed with Kapton and hairspray. I have found that my large prints stick so well that I have to heat cycle the bed to get them to release.
I also have been running the 1st layer temp about 5° hotter than the rest of the print. I have to run my black filament hotter than my red, so it seems that filament temps can vary.
Happy printing