<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Prints Warping and Peeling up]]></title>
		<link>https://www.soliforum.com/topic/3674/prints-warping-and-peeling-up/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/3674/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Prints Warping and Peeling up.]]></description>
		<lastBuildDate>Mon, 26 Aug 2013 10:39:37 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Prints Warping and Peeling up]]></title>
			<link>https://www.soliforum.com/post/34283/#p34283</link>
			<description><![CDATA[<p>Brims, glass, hairspray, first layer speed all help.. The best in my opinion is to make an acetone slurry up and give the bed two coats, in opposing directions.. ;-) 8inch x 5inch print last night... , No brim/raft ---&gt;Zero warp...a brush of acetone on a brim helps hold the corners of the brim down if u want to use the brim route...but really I can&#039;t see past the slurry for those prints u can&#039;t have any warping on.. My 2p!</p>]]></description>
			<author><![CDATA[null@example.com (saymo606)]]></author>
			<pubDate>Mon, 26 Aug 2013 10:39:37 +0000</pubDate>
			<guid>https://www.soliforum.com/post/34283/#p34283</guid>
		</item>
		<item>
			<title><![CDATA[Re: Prints Warping and Peeling up]]></title>
			<link>https://www.soliforum.com/post/34211/#p34211</link>
			<description><![CDATA[<div class="quotebox"><cite>frozensoda wrote:</cite><blockquote><div class="quotebox"><cite>Mr.Factotum wrote:</cite><blockquote><p>Any Suggestions on getting the prints to stick well to the kapton? I am Using Octave White with 195C on the extruder and 95C on the bed. The bed is level and the Z offset is just right, But about a quarter the way into a print one corner will begin to peel up and I kill the print. Any Suggestions?</p></blockquote></div><br /><p>a light coating of hairspray, and setting the brim to 4mm, and setting first layer speed to 60% </p><p>After I did these things I never had another warped print. The hairspray lasts for a long time and you really only need to clean it off when it becomes too thick to be level.</p></blockquote></div><p>+1 on all this.&nbsp; I run my 1st layer speed at 50%&nbsp; On large prints that are a 100mm or more, I set my 1st layer extrusion width to 200% and run a 6mm brim.&nbsp; On prints between 50mm-100mm i&#039;ll use a brim of 4mm.&nbsp; Anything less than that, 1st layer width to 150% and no brim.</p><p>I&#039;m using the stock SD3 bed with Kapton and hairspray.&nbsp; I have found that my large prints stick so well that I have to heat cycle the bed to get them to release.</p><p>I also have been running the 1st layer temp about 5° hotter than the rest of the print.&nbsp; I have to run my black filament hotter than my red, so it seems that filament temps can vary.</p><p>Happy printing</p>]]></description>
			<author><![CDATA[null@example.com (johnforeman)]]></author>
			<pubDate>Sun, 25 Aug 2013 11:25:00 +0000</pubDate>
			<guid>https://www.soliforum.com/post/34211/#p34211</guid>
		</item>
		<item>
			<title><![CDATA[Re: Prints Warping and Peeling up]]></title>
			<link>https://www.soliforum.com/post/34206/#p34206</link>
			<description><![CDATA[<p>Get a piece of glass, use hairspray, heat your bed to 100C (and make sure it reaches that temp before starting) and use a brim.</p><p>It will help but you will still run into the occasional lifting.&nbsp; You may also want to experiment with a raft.</p>]]></description>
			<author><![CDATA[null@example.com (Shotline)]]></author>
			<pubDate>Sun, 25 Aug 2013 04:19:50 +0000</pubDate>
			<guid>https://www.soliforum.com/post/34206/#p34206</guid>
		</item>
		<item>
			<title><![CDATA[Re: Prints Warping and Peeling up]]></title>
			<link>https://www.soliforum.com/post/34205/#p34205</link>
			<description><![CDATA[<div class="quotebox"><cite>Mr.Factotum wrote:</cite><blockquote><p>Any Suggestions on getting the prints to stick well to the kapton? I am Using Octave White with 195C on the extruder and 95C on the bed. The bed is level and the Z offset is just right, But about a quarter the way into a print one corner will begin to peel up and I kill the print. Any Suggestions?</p></blockquote></div><br /><p>a light coating of hairspray, and setting the brim to 4mm, and setting first layer speed to 60% </p><p>After I did these things I never had another warped print. The hairspray lasts for a long time and you really only need to clean it off when it becomes too thick to be level.</p>]]></description>
			<author><![CDATA[null@example.com (frozensoda)]]></author>
			<pubDate>Sun, 25 Aug 2013 04:17:53 +0000</pubDate>
			<guid>https://www.soliforum.com/post/34205/#p34205</guid>
		</item>
		<item>
			<title><![CDATA[Prints Warping and Peeling up]]></title>
			<link>https://www.soliforum.com/post/34204/#p34204</link>
			<description><![CDATA[<p>Any Suggestions on getting the prints to stick well to the kapton? I am Using Octave White with 195C on the extruder and 95C on the bed. The bed is level and the Z offset is just right, But about a quarter the way into a print one corner will begin to peel up and I kill the print. Any Suggestions?</p>]]></description>
			<author><![CDATA[null@example.com (Mr.Factotum)]]></author>
			<pubDate>Sun, 25 Aug 2013 03:37:33 +0000</pubDate>
			<guid>https://www.soliforum.com/post/34204/#p34204</guid>