1

Topic: SD2 extruder doesn't get hot

Hi.
I have a problem with my Solidoodle 2.
After working perfectly well for two months,
now the extruder doesn't get hot.
The trouble happened when I was just printing a model.
SD2 worked fine for a couple of hours, but suddenly
the temperature of the extruder started to go down.
The nozzle stopped extruding because of the low temperature,
leaving the bottom half of the model on the platform.
After that, the extruder never heats itself.
I tried again and again after rebooting my PC and also SD2,
but the extruder never becomes hot.
The platform gets hot, but not the extruder.

The heater of the extruder may be broken.
But I used my SD2 only for two months.
Does the extruder easily be broken?

Can anybody give me any advice?

2

Re: SD2 extruder doesn't get hot

The extruder heater could be burned out... this is a common thing on all 3d printers... do you have any experience in electronics or a volt meter? it also could be just a loose wire connection either at the plug on the print head or where the wires attach to the mainboard.

3

Re: SD2 extruder doesn't get hot

here is a quick link on troubleshooting the extruder ---> http://www.soliforum.com/topic/636/hot- … to-repair/
any other details you can give us on errors or whatnot will be very helpful smile and if you can take some close up pics of the hotend, connectors, mainboard, etc....

4

Re: SD2 extruder doesn't get hot

Thank you for your advice.
Yes, I checked the connectors if it is a problem of loose wires,
but nothing changed.

I read the linked document.
It was very helpful.

I have 12V on the main circuit board.
[img]DSC08257.png[/img]

But not on the red plug of the extruder.
[img]DSC08265.png[/img]

Is this the cause of my problem?
It should be 12V, too?
The red plug of the extruder is the input of the heater, isn't it?

The resistance between the two pins of the red plug of the extruder was 7.3 ohms.
So the heater is alive?
[img]DSC08266.png[/img]

Post's attachments

DSC08257.png
DSC08257.png 3.07 mb, file has never been downloaded. 

DSC08265.png
DSC08265.png 3.02 mb, file has never been downloaded. 

DSC08266.png 3.02 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

5

Re: SD2 extruder doesn't get hot

Sorry, I chouldn't understand how to make links to my photos.
It says that there are too many links.

6

Re: SD2 extruder doesn't get hot

yeah, you need a couple more posts before it will let you post links/photo links

if you got 7 oihms on the heater plug it should be good.

also if you have 12v at the main board out to the extruder heater you should also have it at the red plug... they use IDC (insulation displacement connectors) connectors so you may have to reseat the connectors where they bite through the insulation to get to the wire....or make sure that the wire didn't get burned off underneath the plastic and stretched away from the IDC part.

7

Re: SD2 extruder doesn't get hot

Now my SD2 is working pretty fine!
Thank you so much for all of your help!