Topic: Solidoodle 2 First Layer uneven
So, I recently got and installed a heated build platform after using the non-heated one for several weeks. It is alot better at keeping builds from peeling off, but I have noticed that when i'm printing the first layer, it sometimes makes these weird bumps and ridges that look ugly and cause the extruder to catch on them. I've tried messing with the settings in Repetier-Host with not much success, and i was wondering if you guys had any suggestions.