Topic: Updated fan shroud for mk5 extruder
Hi all,
I've finally gotten this so I'm happy with it. If you have printed 2n2r5's fan for the mk5, then there may not be much point in printing this.
2n2r5's fan:
http://www.soliforum.com/topic/3045/mk5 … -consumer/
This design is quite compact but the airflow from the fan is compromised as a result. It does do the job, however, and print quality is greatly improved when used at an appropriate time.
Instructions
Print parts at high infill for strength. No support needed. The fan shroud (ironically) prints a lot better with a fan. Therefore, you may like to print one, fit it and use it to print another, better quality shroud.
M3 x 10mm bolts to attach the accessory mount to the shroud.
Use a few layers of Kapton tape to protect the inside of the shroud from the heat of the extruder.
40mm fan should slip straight in.
Dimensions in mm.
http://www.thingiverse.com/thing:115659