Topic: Glass bed No Stick
PLA NOT sticking to glass bed
I installed a glass bed on my Ordbot Hadron
Common window glass over heated aluminum bed
using PLA at Extruder temp 185 - 200
bed temps 40 - 90
Glass cleaned with ammonia cleaner
Bare glass tried hair spray on glass tried
First layer being smooshed into bed
Extruded plastic isn't sticking at all
any suggestions?
tnx
Ray