<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Glass bed No Stick]]></title>
		<link>https://www.soliforum.com/topic/440/glass-bed-no-stick/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/440/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Glass bed No Stick.]]></description>
		<lastBuildDate>Wed, 26 Jun 2013 21:07:05 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/28113/#p28113</link>
			<description><![CDATA[<p>assuming you have the correct thermistor table selected, try printing at 175C</p>]]></description>
			<author><![CDATA[null@example.com (Ghostling)]]></author>
			<pubDate>Wed, 26 Jun 2013 21:07:05 +0000</pubDate>
			<guid>https://www.soliforum.com/post/28113/#p28113</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/27440/#p27440</link>
			<description><![CDATA[<p>Blue painters tape or hairspray, or ABS Slurry (ABS Melted into acetone)</p>]]></description>
			<author><![CDATA[null@example.com (mrjohnecker)]]></author>
			<pubDate>Fri, 21 Jun 2013 22:44:13 +0000</pubDate>
			<guid>https://www.soliforum.com/post/27440/#p27440</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/26664/#p26664</link>
			<description><![CDATA[<p>Maybe some hairspray could help !</p>]]></description>
			<author><![CDATA[null@example.com (mcbride19)]]></author>
			<pubDate>Mon, 17 Jun 2013 10:37:34 +0000</pubDate>
			<guid>https://www.soliforum.com/post/26664/#p26664</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/26656/#p26656</link>
			<description><![CDATA[<p>I couldn&#039;t get PLA to glass unless I set the bed temp to at least that of ABS bed temp.</p><p>With zero temperature the PLA sticks nicely to 3M blue tape.</p>]]></description>
			<author><![CDATA[null@example.com (lawsy)]]></author>
			<pubDate>Mon, 17 Jun 2013 09:02:56 +0000</pubDate>
			<guid>https://www.soliforum.com/post/26656/#p26656</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/26654/#p26654</link>
			<description><![CDATA[<p>Before the next print wipe the surface with a disolvent, acetona.</p>]]></description>
			<author><![CDATA[null@example.com (James_T_Menendez)]]></author>
			<pubDate>Mon, 17 Jun 2013 08:45:13 +0000</pubDate>
			<guid>https://www.soliforum.com/post/26654/#p26654</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/3980/#p3980</link>
			<description><![CDATA[<p>I etched the glass top surface with etching cream.</p><p>PLA still won&#039;t stick&nbsp; &nbsp; Extruder temp&nbsp; 200 / 185&nbsp; &nbsp; &nbsp; Bed&nbsp; &nbsp;75 / 25</p><p>Any help?</p><p>Tnx<br />Ray</p>]]></description>
			<author><![CDATA[null@example.com (cozmicray)]]></author>
			<pubDate>Fri, 02 Nov 2012 23:19:33 +0000</pubDate>
			<guid>https://www.soliforum.com/post/3980/#p3980</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/3828/#p3828</link>
			<description><![CDATA[<p>The ABS is good, but PLA can be a different matter.&nbsp; Those who are trying it say that once you get it stuck, it works great, and the reduced cost is worth the effort to get it dialed in.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Thu, 01 Nov 2012 18:50:10 +0000</pubDate>
			<guid>https://www.soliforum.com/post/3828/#p3828</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/3817/#p3817</link>
			<description><![CDATA[<p>Same with me. <br />Still using factory Kapton tape on bed and Solidoodle and Octave abs.<br />And every once in a while I have had to realign my table height after trying to remove super stuck prints even after the bed has cooled down.</p>]]></description>
			<author><![CDATA[null@example.com (HelmutK)]]></author>
			<pubDate>Thu, 01 Nov 2012 18:40:32 +0000</pubDate>
			<guid>https://www.soliforum.com/post/3817/#p3817</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/3810/#p3810</link>
			<description><![CDATA[<p>After having some issues with my Octave ABS at first, I&#039;ve got it dialed in to where I&#039;m having a hard time taking it off the build platform now.&nbsp; Still using factory Kapton tape with rips in it and all.</p>]]></description>
			<author><![CDATA[null@example.com (cmetzel)]]></author>
			<pubDate>Thu, 01 Nov 2012 18:33:46 +0000</pubDate>
			<guid>https://www.soliforum.com/post/3810/#p3810</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/3806/#p3806</link>
			<description><![CDATA[<p>What PLA are you using?&nbsp; Chinese PLA from the likes of RepRaper, Octave, etc have a reputation for being difficult to stick.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Thu, 01 Nov 2012 18:29:45 +0000</pubDate>
			<guid>https://www.soliforum.com/post/3806/#p3806</guid>
		</item>
		<item>
			<title><![CDATA[Glass bed No Stick]]></title>
			<link>https://www.soliforum.com/post/3792/#p3792</link>
			<description><![CDATA[<p>PLA NOT sticking to glass bed</p><p>I installed a glass bed on my Ordbot Hadron<br />Common window glass over heated aluminum bed<br />using PLA at Extruder temp&nbsp; 185 - 200<br />bed temps 40 - 90</p><p>Glass cleaned with ammonia cleaner<br />Bare glass tried&nbsp; &nbsp;hair spray on glass tried</p><p>First layer being smooshed into bed</p><p>Extruded plastic isn&#039;t sticking at all</p><p>any suggestions?</p><p>tnx<br />Ray</p>]]></description>
			<author><![CDATA[null@example.com (cozmicray)]]></author>
			<pubDate>Thu, 01 Nov 2012 17:43:19 +0000</pubDate>
			<guid>https://www.soliforum.com/post/3792/#p3792</guid>
		</item>