I upgraded to Repetier 0.85b and Slicer 0.9.9 and I haven't been able to produce a decent print since.
The last repetier was downloaded from Solidoodle website, and this new version was downloaded from the Repetier website.
The biggest problem I am getting seems to be with too much filament being extruded on the first layers, and then not enough on the outer perimeters (there are visible gaps).
I've tried comparing all my settings in the old software to the new software and they all seem to be the same, and I have even gone as far as printing using the older software versions with the same result.
I have been tearing my hair out for days with this.