Hi is anyone else having difficulty extruding formfortura filament?
I have had no problems with the white and green, but failed missrably with the blue and yellow, i've not dared try the black yet.
I have been extrudeing at solidoodles 195 to 205 with the same results (i have been fine with 195 for the white and green) i beleive solidoodle actual temp is around 35 degree higher then this?
The filament comes out rough and just won't stick or squish flat enough and blocks the nozzle here is a photo of the roughness.
I have tried extruding 50mm prior to printing and its comes out just fine. I've adjusted my depth to platform from squished flat up until its just no being pressed on to the platform at all. All i can think of is the temperature needs to be higher?
Appreciate any advise? The material is brand new.