Topic: Glow in the dark from Makerbot - not enough heat?
I bought some glow in the dark ABS from Makerbot, but I'm not sure it will work.
The problem is in the temperature, I'm trying to print at 210C, but it does look like it's not high enough, the layers are not sticking together.
How high would it be safe to go? (after changing the firmware limit)
For what I found, the first thing to fail would be the PEEK, is it right? Is there anyway around the PEEK melting?