Topic: Iphone Gear Case Print
Anyone get this to print well with slicer?
I realized I needed supports then I got it print ok
But:
1: the supports ruin the print trying to break off of the bottom and then they print on the vertical sides that snap onto the phone. Too much support
2: problem is the floor/back/bottom of the case is about 6 layers up from the bed. This allows the gears to rest flush I assume.
I should just start with simplier things like boxes and covers LOL
I used 0.98 slicr
1.5mm honeycomb support
.45 fill
.3 layer height
I turned on solid layers every 1 and infill every 1
top and bottom solids at 3
perimeters was 4
speed around 35mm/s
I was wondering do i just turn the infill off and print the bottom layer as 7 or 8 layers solid? (that way the floor is solid) everything after 10-47 is just the side walls
it printed well looks were OK not great the solid floor still had lots of little misses. Like the infil didn't touch the edges of the model. The sides came out ok with little to no banding
I think this would be a simpler model and more roboust if it was just one solid piece. Can you print this with gears in place and break them loose?
Print for fun and for parts for my sports cars
current car is 88 IROC