Topic: Davinci 10 A
Hi Guy's
I am having a problem with the filament feeding through my e3d nozzle the aluminum pinch wheel that pinches the filament keeps freezing up i have had it off cleaned it and lubed it but still the same condition is there a replacement for it where could i find one thanks.