Topic: New User - Twisted the Auger Pipe and Stripped a Gear (Resolved)
I just purchased the Filastruder 2.1a kit and assembled it. One pound of ABS was extruded successfully. I purged the ABS and then added the Eastar 6763 PETG pellets and extruded about 20 meters at 190 C this weekend. Then tonight I attempted to extrude more PETG but the filastruder was seriously damaged. I waited for 20 minutes after the temperature reached 190 C and about 2 meters of PETG extruded. The temperature went down to 165 C and the auger pipe started twisting and I could hear the gearbox sputtering. I took it apart and took pictures.