Topic: Hollow print, loose 'skin'.
I printed the Pink Panther Woman, full size, no infill, 4 perimeters, .3 mm layer height. In the curves toward the center, the filament leaves gaps, as can be seen in the photos. What could I do, other than not print it hollow, to prevent this? Also, when the print was done, the z axis moved past 150 mm and kept going, grinding the gears inside the motor until I hastily hit emergency stop. The number for the z axis showed 163. Is there something in the software that I can set so that large prints don't drop the bed past this limit when the print is done?