1

Topic: Hollow print, loose 'skin'.

I printed the Pink Panther Woman, full size, no infill, 4 perimeters, .3 mm layer height. In the curves toward the center, the filament leaves gaps, as can be seen in the photos. What could I do, other than not print it hollow, to prevent this? Also, when the print was done, the z axis moved past 150 mm and kept going, grinding the gears inside the motor until I hastily hit emergency stop. The number for the z axis showed 163. Is there something in the software that I can set so that large prints don't drop the bed past this limit when the print is done?

Post's attachments

photo 1.JPG
photo 1.JPG 615.35 kb, file has never been downloaded. 

photo 2.JPG
photo 2.JPG 597.5 kb, file has never been downloaded. 

photo 3.JPG
photo 3.JPG 513.47 kb, file has never been downloaded. 

photo 4.JPG
photo 4.JPG 521.78 kb, file has never been downloaded. 

photo 5.JPG 662.79 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
...sativas are for smoking!

2

Re: Hollow print, loose 'skin'.

Turn on infill and set it to .1 or something, I think that's the issue.  You're printing unsupported.  Probably could do it with a fan mod too. 

For high prints I edit the gcode file manually to get rid of the last z movement or minimize it.  There's probably an easier way but that works fast and I don't have to mess with any other settings.

3 (edited by nickythegreek 2013-02-21 02:11:17)

Re: Hollow print, loose 'skin'.

I used 5 perimeters, hollow print.

http://www.soliforum.com/post/7072/#p7072

The bed trying to lower itself is something in your end gcode.

4

Re: Hollow print, loose 'skin'.

Since you don't have any inner printing going on it doesn't leave much time for the outer perimeters to cool... so either slowing the print speed down(might not help too much) or the fan mod(I think this would help the most) Also how is it drawing the perimeters? inside to outside or outside to inside? makes a difference on the sloped areas....

5

Re: Hollow print, loose 'skin'.

ronsii wrote:

the sloped areas....

ahh, the sloped areas..

6

Re: Hollow print, loose 'skin'.

Oh... I meant to say the voluptuously rounded areas smile

7

Re: Hollow print, loose 'skin'.

lol...
I was going to do it again, and try 6 perimeters, and still keep it hollow.
And it does print inner to outer. Can this be changed in slic3r??

...sativas are for smoking!

8

Re: Hollow print, loose 'skin'.

creationblur wrote:

lol...
I was going to do it again, and try 6 perimeters, and still keep it hollow.
And it does print inner to outer. Can this be changed in slic3r??


kISSlicer will print from outside to inside I believe.  Might be a solution but you will have to set it up properly.

SD2 with E3D, SD Press, Form 1+
Filastruder
NYLON (taulman): http://www.soliforum.com/topic/466/nylon/