So yeah. More problems. I just upgraded to an e3d v6 hotend and various other mods. I cannot get PLA to stick with the new extruder. I've searched the internet for solutions, but i can only find the same old suggestions. Noted that i have not printed PLA in 3-4 yrs. i got it to sort of stick before on plain fully degreased glass (glass cleaner followed by acetone). This time the best adhesion i can get still allows me to blow the print off the bed while still hot .
I have attempted most permutations of the following:
extruder temp 180-220c
bed temp 50-100c
bed materials:
kapton
plain glass (stripped and dehumidified with both alcohol and acetone)
glue stick on glass (works great for abs)
glue stick "activated" with a water mist
glue stick "activated" with a few drops of acetone.
The bed is as level as i can make it. I bought a dial indicator, but I've yet to figure out a way to mount it with the e3d v6 in the way. I homed the z axis, then did the paper trick (a rather thin piece on purpose), no luck I then homed the z-axis, then ran the gcode to move the bed to .3mm, which is the first layer depth I'm using. I then leveled again with paper. Adhesion was barely good enough to get a calibration cube (poorly.. more like a calibration blob) printed.
This PLA is about 4 yrs old and was not kept in desiccant. Does PLA stop sticking when it gets moist? (a note: my abs was stored in same condition and it prints fine. MAYBe a little steam now and again but no bubbles)