Topic: Thin and weak walls
Hi There,
I've been doing the 3D printing for about a month now. Awesome stuff. I've ran into a problem lately. I'm trying to print a phone case, but the walls are coming out thin,weak and brittle. This is on a Davinci Pro using XYZware for Pro
http://i1053.photobucket.com/albums/s47 … mnvllj.jpg
http://i1053.photobucket.com/albums/s47 … 3tqbrp.jpg
http://i1053.photobucket.com/albums/s47 … g3zbrg.jpg
When trying to pull it off the print bed, they sometimes break off. The weird thin is I had success the first couple of times I printed the case. (I'm pretty sure no setting were changed.) Now the walls are brittle and you can even put your fingernail between the walls and separate them. The wall thickness is 1.6mm. I'm using Hatchbox PLA, .3mm layer height, 200C nozzle/60C bed, and 30mm/s for speed. I seen somewhere to try multiples of .4 (Nozzle width), So I printed a test piece with 3 vertical walls with different thickness(1.2mm, 1.6mm, & 2.0mm). The test printed out fine. Even the thinnest wall at 1.2 mm was fairly sturdy and rigid, although I could still put a fingernail in that one. Why would it work on this test , but not the phone case? Any help would be appreciated.
Thank You, Alex