Topic: Solidoodle 3 Machine Failure at 225 C Extruder Temp

I have a strange issue that is happening. I have an old SD3 and when I update my extruder temp to 225 C my machine will stop print in a 5-10 seconds. This has happened 5 times in a row. I know that the temp shown is off because of poor SD3 design with thermistor location but I find it strange of this happening so often.

2

Re: Solidoodle 3 Machine Failure at 225 C Extruder Temp

MAX TEMP. Cut out on an SD3 is 215 or 220 it's a safety feature to prevent melting the PEEK hot end.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

3

Re: Solidoodle 3 Machine Failure at 225 C Extruder Temp

Not strange at all I had the same issue printing ngen a couple weeks ago setting the temp to lower did the trick.
Tin

Soliddoodle 4 stock w glass bed------Folger Tech Prusa 2020 upgraded to and titan /aero extruder mirror bed
FT5 with titan/ E3D Aero------MP mini select w glass bed
MP Utimate maker pro-W bondtech extruder
Marlin/Repetier Host/ Slic3r and Cura

4

Re: Solidoodle 3 Machine Failure at 225 C Extruder Temp

How can you change that high temp setting for the Max Temp?

5

Re: Solidoodle 3 Machine Failure at 225 C Extruder Temp

You change it by flashing the firmware...but this is not advised unless you upgrade your hot end!

SD2 - Stock - Enclosure - Heated Bed - Glass Plate - Auto Fire Extinguisher
Ord Bot Hadron - RAMPS 1.4 - Bulldog XL - E3D v6 - 10" x 10" PCB Heated Build w/SSR - Glass Plate
Thanks for All of Your Help!

6

Re: Solidoodle 3 Machine Failure at 225 C Extruder Temp

^ that
I'm going to move this out of the XYZ section since it's an SD printer.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

7

Re: Solidoodle 3 Machine Failure at 225 C Extruder Temp

what the others have said...

the MAX temp is set low on stock SD hotends on purpose - to prevent damage to the PEEK liner.

If you want to increase it, it would be best to upgrade to a hotend that can handle it, such as E3D. Both the v6 and the lite6 (budget friendly) are great hotends.

SD4 #1 & #2 - Lawsy carriages, E3D v6, Rumba controller board, mirror bed plate, X motor fan, upgraded PSU & Mica bed heater
SD4 #3 - in the works ~ Folgertech FT-5, rev 1
Printit Industries Beta Tester - Horizon H1

8

Re: Solidoodle 3 Machine Failure at 225 C Extruder Temp

To add to hearless' comment, the ED3 lite while being a great economical hot end is still limited to 230c. and a Ed3 6 is limited to 300c with a thermistor.  Higher temps are required by the high end high strength material such as colorfabb xt , and nylons.

If all you want need to print . is  abs and pla a lite is plenty. Also the colorfab NGeen will print at the upper limit of most printers. 
Tin

Soliddoodle 4 stock w glass bed------Folger Tech Prusa 2020 upgraded to and titan /aero extruder mirror bed
FT5 with titan/ E3D Aero------MP mini select w glass bed
MP Utimate maker pro-W bondtech extruder
Marlin/Repetier Host/ Slic3r and Cura

9

Re: Solidoodle 3 Machine Failure at 225 C Extruder Temp

Points of clarification the E3d Lite6 is good up to 250 degrees.
The regular V6 can handle temps higher than 300 degrees if properly equipped with a thermal couple.  Regular thermistors fail at just above 300 degrees but the V6 is just fine.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

10

Re: Solidoodle 3 Machine Failure at 225 C Extruder Temp

Sorry ward for the mis info on the lite.  and failed to mention the thermocouple option.
Tin

Soliddoodle 4 stock w glass bed------Folger Tech Prusa 2020 upgraded to and titan /aero extruder mirror bed
FT5 with titan/ E3D Aero------MP mini select w glass bed
MP Utimate maker pro-W bondtech extruder
Marlin/Repetier Host/ Slic3r and Cura

11

Re: Solidoodle 3 Machine Failure at 225 C Extruder Temp

No need to apologize smile

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions