Bed temps should stay the same (you haven't changed anything there!). For ABS it seems 90-100C is often advised.
Extruder temp will change: the solidoodle stock hotends measure temperature in a different place to the E3D hotends. For ABS, the E3D will tend to be happy somewhere between 230 and 240C (which you'll note is a bit higher than the stock hotend temps, generally recommended 205-220C).
Of course, depends quite a lot on the filament, a little bit on the print speed, so experiment and see how you go.