Topic: Budget Enclosure
To solve an issue with warped long parts I've decided to enclose the SD2 to keep the ambient temperature up. I'm happy to say that it worked like a charm. In fact, on the next run I'm going to lower the bed temp from 105 (glass bed) back to 95 cause after I removed the part from the bed it warped slightly UP in the middle (usually it's been the other way around). I figure that the layers near the bed were kept too warm and they contracted after cooling off the bed.
For the enclosure I improvised with a box and some packing tape.