To solve an issue with warped long parts I've decided to enclose the SD2 to keep the ambient temperature up. I'm happy to say that it worked like a charm. In fact, on the next run I'm going to lower the bed temp from 105 (glass bed) back to 95 cause after I removed the part from the bed it warped slightly UP in the middle (usually it's been the other way around). I figure that the layers near the bed were kept too warm and they contracted after cooling off the bed.

For the enclosure I improvised with a box and some packing tape.

Post's attachments

2013-01-24 10.49.17.jpg
2013-01-24 10.49.17.jpg 1.79 mb, 2 downloads since 2013-01-24 

2013-01-24 10.49.25.jpg
2013-01-24 10.49.25.jpg 1.89 mb, 3 downloads since 2013-01-24 

2013-01-24 10.49.32.jpg
2013-01-24 10.49.32.jpg 2.16 mb, 2 downloads since 2013-01-24 

You don't have the permssions to download the attachments of this post.

2

Re: Budget Enclosure

mm2tts wrote:

To solve an issue with warped long parts I've decided to enclose the SD2 to keep the ambient temperature up. I'm happy to say that it worked like a charm. In fact, on the next run I'm going to lower the bed temp from 105 (glass bed) back to 95 cause after I removed the part from the bed it warped slightly UP in the middle (usually it's been the other way around). I figure that the layers near the bed were kept too warm and they contracted after cooling off the bed.

For the enclosure I improvised with a box and some packing tape.

I have the metal case and it gets warm. I'm running my bed at 70c and believe I can go much lower in time.

3

Re: Budget Enclosure

mm2tts wrote:

To solve an issue with warped long parts I've decided to enclose the SD2 to keep the ambient temperature up. I'm happy to say that it worked like a charm. In fact, on the next run I'm going to lower the bed temp from 105 (glass bed) back to 95 cause after I removed the part from the bed it warped slightly UP in the middle (usually it's been the other way around). I figure that the layers near the bed were kept too warm and they contracted after cooling off the bed.

For the enclosure I improvised with a box and some packing tape.



That sure is a budget enclosure...The window made of tape is a nice touch...

SD2 with E3D, SD Press, Form 1+
Filastruder
NYLON (taulman): http://www.soliforum.com/topic/466/nylon/

4

Re: Budget Enclosure

I've removed my metal enclosure and replaces with card taped to the frame. cardboard seems to keep the heat better.

5

Re: Budget Enclosure

Yes, corrugated cardboard is insulated by default!

6

Re: Budget Enclosure

kind of annoying that I paid for an enclosure when a better enclosure came free with the machine, (the shipping box)

7

Re: Budget Enclosure

I love your "enclosure", seriously ghetto looking, but a great idea. I bet it does get nice and toasty in there. I don't have the shipping box any more, other wise I would do that too. I have to admit, I LOL'd pretty hard when I saw the first picture of your enclosure. I was expecting card board panels to be adhered to the printer, but just slipping the entire box over like a big glove is way better!

8

Re: Budget Enclosure

This thread gave me an idea for an enclosure. I decided to cut up the shipping box and make some walls. Then I attached them with some brown packing tape. Its not going to win any beauty contests but it keeps heat in.

Post's attachments

solid-box.png
solid-box.png 1.11 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

9 (edited by iowajames 2013-04-29 14:14:49)

Re: Budget Enclosure

Really, if it works. Good job dude.

No trees were harmed in the creation of this email, though some electrons were horribly inconvenienced.