51

Re: XYZ PLA now available

I order to print with PLA you need to have 2 x PLA carts installed.  It will not allow you to use with 1 x PLA and 1 x ABS cart installed.  Ridiculous and another reason I sent my 2.0A Duo back today.  Just too may restrictions.

52

Re: XYZ PLA now available

Ahh that explains it. So I need two of the same colors because I have yet to find a different color of PLA in cart form. SMH. Thats so stupid. I really wish I hadn't gotten this POS! Mine is still under warranty but out of return time to amazon. They XYX sent me a free new print head but failed to tell me that I needed two freakin PLA carts. I called them several times and they keep blowing me off. This company should not be able to sell on Amazon at all.

53

Re: XYZ PLA now available

xyz recently sent me a replacement Da Vinci 1.0A and it came with the upgraded extrude, it took a while for it to load the PLA filament but once it got started it just works.