Topic: davinci 1.0 rod shaft bend :(
I bought a used printer,
I now understand why I buy cheap!
I had much difficulty in calibrating my printer!
I buy this: http://www.banggood.com/0_01mm-Accuracy … 48936.html print this http://www.thingiverse.com/thing:718768 and I realized now my problem!
please look : https://youtu.be/niw1ZFHhfv4
I have the same problem with the left, but can very
please help !
it is possible to repair the problem or should I change?
if I should change or even find parts?
thank you for your help
firmware repetier