Filament: Biopolymer by 3Dom (?)
Extruder temp: 250º C
Bed temp: 90º C
Software: Soliprint
Layer height: 0.3mm
Rating: 3/10
I am not convinced that I actually got the right material from globalFSD on this one. Supposedly it is Ingeo, or a kind of PLA, but I couldn't get it to extrude at all until I hit about 230º, and that was with some help. It does extrude pretty well at 250º, but the layer adhesion is very poor, and it doesn't seem particularly strong. It also shrinks a lot as it cools, and was moderately difficult to get stuck to the bed.
The good news is that I couldn't detect any odor what so ever as it was printing. It didn't smell sweet like PLA, or harsh like ABS. It just didn't smell like anything.
In short, it prints pretty well at high temps, but doesn't have very good mechanical properties.
Post's attachmentsIMG_0117.jpg
IMG_0117.jpg 33.65 kb, file has never been downloaded.
IMG_0118.jpg
IMG_0118.jpg 33.65 kb, file has never been downloaded.
IMG_0119.jpg
IMG_0119.jpg 35.83 kb, file has never been downloaded.
You don't have the permssions to download the attachments of this post.