1

Topic: Glass bed for Flashforge Dreamer

Here is my installation, you need:

- 1/4" thermal Glass from Flashforge 6"x9"x1/4"
- Some kapton tape 5mil self-adhesive (cut 4 pieces 1/2" x 6")
- Some blue paint tape
- 6.5mm flashforge shim for Z axis (Search thingverse site... thing:427689 )

See my pictures for the installation.

Everything must be very clean before installing the glass bed... use a little bit of aceton to clean...

It prints great with UHU glue stick. Easy to apply, easy to wash...

No binder clips needed... No danger for extruders or the 3D printer...

Post's attachments

IMG_2053.JPG
IMG_2053.JPG 281.96 kb, 3 downloads since 2014-09-20 

IMG_2055.JPG
IMG_2055.JPG 276.8 kb, 2 downloads since 2014-09-20 

IMG_2056.JPG 278.4 kb, 2 downloads since 2014-09-20 

IMG_2057.JPG
IMG_2057.JPG 293.96 kb, 2 downloads since 2014-09-20 

IMG_2058.JPG
IMG_2058.JPG 340.75 kb, 2 downloads since 2014-09-20 

You don't have the permssions to download the attachments of this post.