1

Topic: Printing off the bed after update.

I got my printer up and running after a few weeks of downtime and noticed a Repetier update. Now whenever I print, the extruder tries to print way off of where it is supposed to be. It keeps hitting the end stops and it seems as though it has no idea where center is. Manual controls work fine. I've looked through all the settings and can't see what it could be. What changed and how do I get it back?

2 (edited by AZERATE 2014-08-31 20:47:13)

Re: Printing off the bed after update.

It could be the printer dimensions under Printer Settings.
Worst case, you could always go to the RH site and reinstall the last version that worked best for you.

Printit Mason and Printit Horizon printers
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

3

Re: Printing off the bed after update.

I checked all that. Nothing seems out of the ordinary.

4

Re: Printing off the bed after update.

I changed the "print center" in Slic3r from 75 x 75  to 0 x 0. Thant worked. Seems weird because I don't remember changing that, or, it worked fine before the update. Whatever. It works now.