Topic: switched to PLA now extruder clicks
I have been using ABS so far, and today decided to switch to some PLA for a try. After switching, now when printing the PLA my extruder is clicking/grinding/squeaking HOWEVER it is not "skipping" like it was clogged or anything.
Did I switch wrong? I extruded the remaining ABS out of the nozzle using 200c while pushing the PLA through and when it started turning the color of the PLA I lowered the temp down to 160 as suggested.
While printing at 160c the extruder is clicking (NOT SKIPPING, I watched it) and even boosting the temp up to 180c, it still made the clicking/squearking noise. I did notice at 180c the PLA printed a more correct color (it was clear PLA and it looked more clear on the finished product with the layers that were 180c) however the 180c also blobbed more.