Topic: getting to print good .1 prints
so, I have a good setting with the stock program for solidoodle 3 that is on solidoodle's website.
but I run a lot of stuff through kisslicer,how do I set that up so its proper with what my settings are in reptierhost?
do I calibrate the same way as .3 on repetier host. with printing a box and checking the wall thickness, if so what should the wall thickness be for .1 prints, (for .3 prints wall thickeness should be .42)
let me know if im confusing or if I missed something.
thankyou.