1

Topic: Replaced z coupler now need original nut holder

so i had banding, and i tried a few fixes but nothing seemed to solve it.  i bought an aluminum flexible shaft coupler you can get on ebay for a few dollars to replace the terribly designed pressed z axis coupling, and now while the first 8 or so layers are great, the  layers start getting progresively worse and worse(banding wise) after that and progressively delaminate easier and easier, and i think its due to a previous fix i installed (that slightly allows a nut to move only in x and y axis) coupled with the flexible coupling.  I unfortunatley discarded the stock z axis nut holder.  The question is does anyone have the files to replicate the stock z axis nut holder? i dont need any anti backlash designs, just the stock simple one.  its a solidoodle 2 pro wood platform.

2

Re: Replaced z coupler now need original nut holder

I might still have one at home -  will check later today for you.

Where are you located?

3

Re: Replaced z coupler now need original nut holder

im on long island in NY.  That would be great!

4

Re: Replaced z coupler now need original nut holder

This what your looking for?  PM your address and I'll get it out in the mail as soon as I can dig out tomorrow wink

Post's attachments

photo.JPG
photo.JPG 323.16 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.