Topic: Smooshing and Plowing
I can't get my Orbot Hadron to print anything nicely?
Here are clear ABS prints ET 200 BT 85
Repetier 070
Looks like I have z axis calibration problem this is using 2760 steps/mm
done by calibration
Any suggestions
Top of peg seems to get smooshed
I can't get my Orbot Hadron to print anything nicely?
Here are clear ABS prints ET 200 BT 85
Repetier 070
Looks like I have z axis calibration problem this is using 2760 steps/mm
done by calibration
Any suggestions
Top of peg seems to get smooshed
Peg_226.jpg
Smooshed Peg
Bottom of cup gets plowed away
Cup241.jpg
Bottom of cup gets plowed
Cup245.jpg
Plowed bottom of cup