I have been running my SD2 for a few days now and I don't see any Z banding. Is it a random problem on random machines? Curious.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Solidoodle Discussion → So not every machine has Z banding?
I have been running my SD2 for a few days now and I don't see any Z banding. Is it a random problem on random machines? Curious.
I think it has to do with how well and centered your z-rod was attached to the stepper. My printer never seemed to have the z banding issue even though it had lots of other problems.
I didn't think I had z banding really until I started printing smaller layer heights. try just printing a 20mm Tube using spiral vase. that should show you if you have any.
I ran an inch tall thin walled cylinder today at.1mm. Looks great!
I didn't see Z banding in the beginning because my quality wasn't that good to begin with. I had moire, backlash, not perfectly calibrated flow rate etc., so the z-banding wasn't noticeable. Fixing other problems and printing smaller layers made it start to show up.
sweet! I guess you can consider yourself lucky. :-)
I found mine degraded as time went on. I found my first few prints in a box and they were fantastic, and the latest prints were pretty average. I soon after swapped to an m5 rod.
I found mine degraded as time went on. I found my first few prints in a box and they were fantastic, and the latest prints were pretty average. I soon after swapped to an m5 rod.
I found the same thing on mine. I have done a few things to remedy the banding without replacing the rod yet but im thinking thats in my near future. Im trying to get through another couple projects before i tear it down for a good rebuild.