Topic: Warping on prints int he same place time after time.
Hi Guys,
Would love any ideas you have about an issue I am having.
When I print, it seems that there is a "dead spot" on my heated bed. Time after time, I get prints that seem to lift and warp as they are printing.
I originally started printing in PLA, and when I was printing hollow prints, I would find that they had lifted, and popped off, being dragged around the print bed. I originally thought this was due to the base not having enough to grip, but soon realised I was not heating the bed to the sufficient temperature.
I recently started printing in ABS, and the issue has gotten worse. Attached are some images of a hollow cylinder I printed. in the "dead zone" the print had lifted and warped the side. If I move the print away from the "dead zone" most times I come out with a perfect print. The issue with that is that the "dead Zone" is near the middle of my print bed. If the part is small enough, I can move it before generating G-Code, but thats not the real issue. ![]()
I have built walls for my Soliddoodle, to see if it might have been cold are affecting the prints, but I get the same results. As I was writing this, I ran another test, of two parts printing, and you can see the warpage on the left part in the "Dead Zone."
This is really frustrating, and I have started not to enjoy my printer, which is not that old. I have no idea if its user error, or if its a fault in the machine itself.
Would really love any ideas, thoughts, ext about what I have described. It's slowly driving me up the wall...
Thanks in advance...
-Skyler101