Topic: Ben Franklin bust
Sd2 at .1mm
Acetone vapor bath
Finished with Rustoleum "Oil Rubbed Bronze" spray paint.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → STL Sharing & Print Showoff → Ben Franklin bust
Sd2 at .1mm
Acetone vapor bath
Finished with Rustoleum "Oil Rubbed Bronze" spray paint.
Looks awesome. Couldn't see any layering in that photo. Very professional results. What equipment are you using for your vapor bath?
Thanks,I use a Presto Kitchen Kettle
http://www.amazon.com/Presto-06006-Kitc … hen+kettle
I learned about it from Ian's blog: http://solidoodletips.wordpress.com/201 … -finisher/
At .1mm there was very little layering,it only took 20secs in the vapor bath to get that result.You can get close to the same at .3 layers but it's best to do multiple exposures at 20-30 sec at a time.
I've seen Ian's method. It is on my list of things to get. Just wanted to see if you were doing something similar, or using a different method. Your print came out awesome.
Can you purge them in water to stop the acetone from eating the plastic between exposures?
+1 for the presto parts finisher!