I just switched to a new roll of filament in mid print, as my old roll was running out. The original roll was white ABS (I don't remember the brand, and the new roll was also white filament but Octave brand.
The switch went on without any glitches, the printer continued where it left off, went on for a few paths, then started to lay down some brown filament. I then noticed I could see smoke from the tip of the extruder, something I hadn't seen before. The filament it was putting down was actually burnt.
I lowered the temperature, and the brown started going away, but by now the print was ruined.
I had previously used pink colored Octave filament and didn't have this problem. Does anyone else use Octave filament and have you come across similar problems, what extruder temps are you using with it?
BTW, my original default temps were 200°C (205° first layer). To get this to stop burning the filament, I had to lower it by 10°, to 190°C.