I have gotten past most of my issues with material not sticking and so on. Here is my latest print. The perimeter walls are horrible, however the floor could not be more perfect.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Help/Repair/Maintenance → Help: Bad perimiter walls
I have gotten past most of my issues with material not sticking and so on. Here is my latest print. The perimeter walls are horrible, however the floor could not be more perfect.
yep.. not enough plastic... your flowrate is too low