Topic: abs melting point
Just curious why we use such a high hotend temp when the melting point of ABS is 105 C
221°F (105°C)
Acrylonitrile butadiene styrene, Melting point
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Solidoodle Discussion → abs melting point
Just curious why we use such a high hotend temp when the melting point of ABS is 105 C
221°F (105°C)
Acrylonitrile butadiene styrene, Melting point
Just curious why we use such a high hotend temp when the melting point of ABS is 105 C
221°F (105°C)
Acrylonitrile butadiene styrene, Melting point
The *glass transition temperature* is 105C. That's the temperature it begins to soften. It is amorphous, and therefore has no true melting point.
From my experience, not all ABS is the same so you really cant use exact numbers to have exact results. Plus, the environment makes a big defference in your settings as well. Best thing to do is test for yourself and go with what works best for you.