Last night I connected the printer and while everything looked fine, and appear to be properly calibrated, I could not get the filament to stick to the build platform no matter what I tried.

I heated the bed to 95°C before printing, cleaned the surface with alcohol to make sure there were not fingerprints, etc.  The printer would start printing, but the first layer wouldn't stick at all, and when the second layer came around, it would just lift the first one off the surface and just mangle it around.

I tried adjusting  the Z limit screw from almost no pressure to too much pressure, but no luck.  I also tried different extrusion temperatures (205°C for the first layer, 200° for the rest), no go.  I was using both the ABS that I bought, and the sample ABS that came with the printer.

Ultimately I ended up using some hair spray, and that worked perfectly.  IN fact I had a bit of a hard time removing the print from the platform once it was done. 

Question: should I remove the print while the platform is still hot, or should I wait for ti to cool off first?

Anyway, here is a picture of my first test.  Not the most accurate or clean, but not bad for a first.. I think

Post's attachments

pooh_test.jpg
pooh_test.jpg 89.56 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
To print or, 3D print, that is the question...
SD3 printer w/too many mods,  Printrbot Simple Maker Ed.,  FormLabs Form 1+
AnyCubic Photon, Shining 3D EinScan-S & Atlas 3D scanners...
...and too much time on my hands.

2

Re: My first object

It should cool down to about 60 and then the print should pop right off.

You have some calibrations ahead of you, nut nice to see it up and running.
i would suggest the flow rate calibration first and then try the same print again.

3

Re: My first object

search for glass + hairspray method. Faster and better than just putting hairspray straight on the bed.

SD2 - Glass Bed, Fans on PCB and Y motor, Custom enclosure