1

Topic: Simple Plexiglas Bed

So, I bought this old DaVinci Jr Wifi a while ago and the previous owner made a mod, which i replicated. Its really simple;

You make four small corners that attach to the existing bed, with screws, and install a precisely cut piece of semi-flexible plexiglas. On top of this, you can put anything you want; I've used BuildTak here in the picture (and with residue glue).

https://images2.imgbox.com/fd/72/pgwWDEb1_o.jpg

Previously, BuildTak was gripping too much on my models, and if it was on top of the glass-plate on the Davinci bed, almost impossible to get out. Also, using a spatular, I had to use so much force I thought i might break the entire printer. However, with this, I just take off the plexiglas, and bend it just enough, to the models to loosen its grip.

There is a small bend in the plexiglas on the above image, from what i do think is when the materials contract - either that or I just forgot to "unbend it" last time i used it (i tend to bend it flat from time to time). However it has never caused an issue with my prints.

Really really simple mod, seen here below - just four pieces. I can find the .stl's as soon as i get access to my old computer again smile

https://images2.imgbox.com/3b/f5/MquvxEiR_o.jpg

2

Re: Simple Plexiglas Bed

If you can send me the measurement of the bed I can draw up the corners. One measurement I can get from the picture.

3 (edited by Woody565 2018-01-28 12:14:09)

Re: Simple Plexiglas Bed

I have done something similar to me mini.

Got a piece of 4mm glass cut to the size of the bed, driller the glass and the original bed with a 5mm hole and used appoxy to secure 5mm rare earth magnets into all holes.

I had to print a 5mm shim to raise the z axis end stop to allow for the extra 5mm added to the build plate.

Stuck a sheet of buildtak on the glass and to be fair that stuff is awesome. Since doing the mod my prints have improved 10 fold and removing the parts is a lot easier now I can remove the build plate.

https://image.ibb.co/e6q21w/2_B33_E68_C_FC6_A_447_D_BCB1_E5_D6171_BAF13.jpg

https://image.ibb.co/cGBLob/AC090074_DE19_40_ED_A688_491798658_BC9.jpg

https://image.ibb.co/crZUgw/3_A1058_BF_23_EF_4_DC9_9_AAB_54_CE577973_AE.jpg

https://image.ibb.co/bBq21w/4_B37_C46_A_9_EA8_4184_B44_E_CACB78_B77506.jpg

4 (edited by bushy 2018-01-28 15:04:11)

Re: Simple Plexiglas Bed

Look good. Appears the Mini has a stronger bottom plate then the Jr.

Edit* let me rephrase that. Not stronger but flatter and more supportive over the whole plane.