1

Topic: HELP PLIS! Barrel Rotate !

Hi,

I need help, I turn on the heatter and wait till get the right temperature , but then when i turn on moter, the barrel start to spin!

2

Re: HELP PLIS! Barrel Rotate !

miguel_puebla_3 wrote:

Hi,

I need help, I turn on the heatter and wait till get the right temperature , but then when i turn on moter, the barrel start to spin!

Once it gets up to temp, are you letting it sit at temp? Have you performed your PID tuning?
Let it sit to temp for about 15-20min

Printit Mason and Printit Horizon printers
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

3

Re: HELP PLIS! Barrel Rotate !

Thanks! Was that thing. hmm.

I thing im yo eager to  start struding