Topic: HELP PLIS! Barrel Rotate !
Hi,
I need help, I turn on the heatter and wait till get the right temperature , but then when i turn on moter, the barrel start to spin!
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Filastruder → HELP PLIS! Barrel Rotate !
Hi,
I need help, I turn on the heatter and wait till get the right temperature , but then when i turn on moter, the barrel start to spin!
Hi,
I need help, I turn on the heatter and wait till get the right temperature , but then when i turn on moter, the barrel start to spin!
Once it gets up to temp, are you letting it sit at temp? Have you performed your PID tuning?
Let it sit to temp for about 15-20min
Thanks! Was that thing.
.
I thing im yo eager to start struding