Topic: First semi successful print (my cube is rectangular)
Hi all,
I just finished my first print that I let run all the way on my workbench apprentice. I believe that I have my extruder calibrated decently. The first few layers are a little dicey - I think my extruder may have caught some of the glue which caused it to get messy, may be over extrusion though. Anyways - My 20mm cube print seems to be rectangular on my x axis and I am curious as to what process I can run through to ensure that my X and Y movements are calibrated?
Greatly appreciated,