1

Topic: da vinci 1.0a with repetior

my extruder stops pushing filament at different points during prints
i can push the reload and it seems to push filament again but it stops when it continues print

any ideas what i can check?
with using other brand filament where do you guys feed it thru to feed the extruder?

Thanks for your help

Dan

2

Re: da vinci 1.0a with repetior

I drilled a small hole in the center of my top and feed from an overhead shelf. As for the stopping check the temp, could be too low and the 1.0 cannot use PLA without mods. So if using PLA, could also be your issue.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: da vinci 1.0a with repetior

i am using abs with 225c settings

4

Re: da vinci 1.0a with repetior

Then watch during the print and when you see it stop, note the temp displayed. You could have a faulty connector on the heater like so many 1.0 machines had.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.