1

Topic: switched to repeater and extruder won't heat

Ive tried everything. Every software version of repetier and still nothing . Its not my wire connector and I have voltage. I can manually set the temp on the extruder will printing. Also its not in dry run. Does anyone have any ideas for me to check? Also my    g code says its telling to heat but nothing. Ive seen other people had this problem and fixed it but didn't come back and tell how they did that.

Here is my g code

Post's attachments

help.gcode 1.15 mb, 1 downloads since 2016-02-20 

You don't have the permssions to download the attachments of this post.

2

Re: switched to repeater and extruder won't heat

Does your printer have a heated bed? If your printer doesn't have a heated bed but you haven't specified this in repetier host then the software won't start heating the extruder until the bed is heated (which never happens as you don't have one obviously)

What you need to do is switch the bed temperature to 0. (I think this is how we solved it)

Hope this helps!

Cheers,
www.3dexfilament.co.uk

3Dex - Suppliers of the best filament.
http://www.3dexfilament.co.uk

3

Re: switched to repeater and extruder won't heat

Sorry I have a da Vinci 1.0 so yes a heated bed. Anything else?

4

Re: switched to repeater and extruder won't heat

So the extruder won't heat up until the bed is fully heated?

5

Re: switched to repeater and extruder won't heat

Yep that's how it works. Man l sent hours on this lol.

6

Re: switched to repeater and extruder won't heat

So have you got it working??

3Dex - Suppliers of the best filament.
http://www.3dexfilament.co.uk

7

Re: switched to repeater and extruder won't heat

Yes there was nothing wrong with it.  I just had to wait to let the bed heat up first

8

Re: switched to repeater and extruder won't heat

Ok well I'm glad you now have it all working! Happy printing

3Dex - Suppliers of the best filament.