Thanks, I deleted them. The server was struggling this morning when I posted.
Here is the thing... I spent hours last night troubleshooting, even took the whole head apart, cleaned it, and refit the thermistor. Delamination with every print in the last 24 hours since resetting the cartridge.
I had about 20 hours of printing with other filaments, all working decently well with the original filament cartridge still in.
I reloaded the filament from the cartridge and reset it to the stock temperatures, but still, poor, brittle, delaminated prints.
So then, I opened up another XZY cartridge that I have, and loaded the filament. Immediately, the keychain print worked great. Loaded 3rd party filament, and now everything prints fine.
It is most certainly something in the EEPROM of the reset cartridge that is messing up prints with the 1.0A on 1.0.1 firmware.
There is something else that needs to be reset, other than the filament length, bed temp, and extruder temp... The post that I referenced in OP stated that he had the same problem until he downgraded the FW on his 1.0, which is not an option with the 1.0A.
Does no one use stock firmware anymore???? LOL
Regardless, I know the solution here is to flash repetier, but I was hoping to solve this problem before I tackle that.
Da Vinci 1.0a. Repetier 0.92. E3D V6. Titan Extruder. Sllic3r. Octoprint on Raspberry Pi B+.