1

Topic: Da Vinci Barrel Length

Does anyone know the barrel length by chance? I need to replace mine and I'm looking at something like this. I just need to make sure it's long enough.  I don't really want to take it apart to find out the length. Looking at something like this http://tinyurl.com/j692cz3.

Thanks.

2 (edited by scobo 2015-12-16 09:00:12)

Re: Da Vinci Barrel Length

Do yourself a favour and replace it with an E3D.
My stock nozzle started showing signs of becoming worn recently so I replaced the whole hotend with an E3D Lite.
My only regret is not doing it sooner. Printing with PLA is now a complete breeze instead of fighting the heat-creep issues with the stock hotend.

Davinci 1.0 with repetier firmware & E3D V6 Lite
Anycubic Photon DLP printer, Einscan-S 3D scanner
Simplify3d, 123D Design, Meshmixer
http://www.thingiverse.com/scobo/designs

3

Re: Da Vinci Barrel Length

Can't replace two different threads on the barrel

Da Vinci  AiO with firmware 1.1.1 using xyzscan 1.1.18
E3Dv6 hotend with custom carriage with Borosilicate glass bed
123D Design and Simplify3D, Replaced PS with a Solidgear Flex320
Zerokart resetter,  Installed a Extruder Controller for higher temps