<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Da Vinci Barrel Length]]></title>
		<link>https://www.soliforum.com/topic/13101/da-vinci-barrel-length/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/13101/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Da Vinci Barrel Length.]]></description>
		<lastBuildDate>Thu, 17 Dec 2015 21:28:47 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Da Vinci Barrel Length]]></title>
			<link>https://www.soliforum.com/post/111970/#p111970</link>
			<description><![CDATA[<p>Can&#039;t replace two different threads on the barrel</p>]]></description>
			<author><![CDATA[null@example.com (kev0175)]]></author>
			<pubDate>Thu, 17 Dec 2015 21:28:47 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111970/#p111970</guid>
		</item>
		<item>
			<title><![CDATA[Re: Da Vinci Barrel Length]]></title>
			<link>https://www.soliforum.com/post/111740/#p111740</link>
			<description><![CDATA[<p>Do yourself a favour and replace it with an E3D.<br />My stock nozzle started showing signs of becoming worn recently so I replaced the whole hotend with an E3D Lite.<br />My only regret is not doing it sooner. Printing with PLA is now a complete breeze instead of fighting the heat-creep issues with the stock hotend.</p>]]></description>
			<author><![CDATA[null@example.com (scobo)]]></author>
			<pubDate>Wed, 16 Dec 2015 08:57:47 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111740/#p111740</guid>
		</item>
		<item>
			<title><![CDATA[Da Vinci Barrel Length]]></title>
			<link>https://www.soliforum.com/post/111696/#p111696</link>
			<description><![CDATA[<p>Does anyone know the barrel length by chance? I need to replace mine and I&#039;m looking at something like this. I just need to make sure it&#039;s long enough.&nbsp; I don&#039;t really want to take it apart to find out the length. Looking at something like this <a href="http://tinyurl.com/j692cz3.">http://tinyurl.com/j692cz3.</a></p><p>Thanks.</p>]]></description>
			<author><![CDATA[null@example.com (craigunderhill)]]></author>