1

Topic: Netfab repairs not doing anything

I have tried lots of times to use the inverted shells repair app in Netfab like Pirvan showed in a tutorial on this site. but it never does any repair other than once it closed an opening that I did not want closed and its not supposed to do that during that repair.

I have the freeware version but must be something missing or disabled on mine. also that repair is not shown i n the list with the others but only in the pull down menu. it goes through the motions but does nothing any way that I try options.

Solidoodle 2 with Deluxe kit cover & glass bed with heater. and 2nd board SD2 used not 3rd and alum platform not installed yet still wood. also need cooling fan installed to board. use Repetier Host couple vers. Slic3r also have all free ware STL programs

2

Re: Netfab repairs not doing anything

n2ri wrote:

I have tried lots of times to use the inverted shells repair app in Netfab like Pirvan showed in a tutorial on this site. but it never does any repair other than once it closed an opening that I did not want closed and its not supposed to do that during that repair.

I have the freeware version but must be something missing or disabled on mine. also that repair is not shown i n the list with the others but only in the pull down menu. it goes through the motions but does nothing any way that I try options.


Try the online version. it is the most up to date and accurate.

https://modelrepair.azurewebsites.net/

It does require a microsoft account.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Netfab repairs not doing anything

no accounts

Solidoodle 2 with Deluxe kit cover & glass bed with heater. and 2nd board SD2 used not 3rd and alum platform not installed yet still wood. also need cooling fan installed to board. use Repetier Host couple vers. Slic3r also have all free ware STL programs

4

Re: Netfab repairs not doing anything

In some occasions I've found repair doesn't help. In such an occasion, I've had to clean up the design and rework it to slice properly. Try cleaning up the lines and save it as another file like "_ _ _ rev2" and see if it helps.

If it does not, then share the original here. If someone doesn't beat me to it, I will take a stab at it between tomorrow and tuesday.

Printit Mason and Printit Horizon printers
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

5

Re: Netfab repairs not doing anything

its lots of stl files with spots/parts inverted (red when viewed, then green when selected for repair). was just wondering why this feature dont work at all on my Netfab. like it does for others

Solidoodle 2 with Deluxe kit cover & glass bed with heater. and 2nd board SD2 used not 3rd and alum platform not installed yet still wood. also need cooling fan installed to board. use Repetier Host couple vers. Slic3r also have all free ware STL programs

6

Re: Netfab repairs not doing anything

seems over 95% of all 3D file sharing sites stl files are in much need of repair or complete redesigning due to so many people having no clue how to create usable files. many files would be easier to just delete and start over from scratch having thousands of errors. and this conclusion was reached after downloading over 10,000 STL files. so thats pretty bad free lance 3D design. also about 15% of those files are not worthy of printing even if possible due to what they are and being unable to do job intended or items available much cheaper already. so use caution when browsing such sites (every known public 3D file repository on the web. and some are spammers pushing malware so careful and use firewall with antivirus).

Solidoodle 2 with Deluxe kit cover & glass bed with heater. and 2nd board SD2 used not 3rd and alum platform not installed yet still wood. also need cooling fan installed to board. use Repetier Host couple vers. Slic3r also have all free ware STL programs

7 (edited by n2ri 2015-08-30 07:09:46)

Re: Netfab repairs not doing anything

Netfab is my fav stl file tweaking app of all the ones I have even with its odd quirks sometimes. but still learning them. a couple others do some repairs etc better/easier I found. still wishing I had another style 3D printer for support free fine detailed tiny models I have that have details at least as good as my metal/resin cast ones. I am nearly as close to replacing my older casting methods with 3D printing as digital cameras come to film type cameras, other than production speed.

Solidoodle 2 with Deluxe kit cover & glass bed with heater. and 2nd board SD2 used not 3rd and alum platform not installed yet still wood. also need cooling fan installed to board. use Repetier Host couple vers. Slic3r also have all free ware STL programs