Here is a print of a Warren Stratford figurine.
This is one of a few Stratford figurines I have scanned using the Atlas 3D scanner. As I have mentioned in my post in the Atlas section the scanning process isn't perfect, but with a little bit of work, you can end up with a model that is very close to the original.
Here is the print of the Fireman next to the original. It was printed in 2 halves @ .1mm. Sliced with Cura, support generated by Meshmixer. No retouching was done, only the supports were removed.
SD3 printer w/too many mods, Printrbot Simple Maker Ed., FormLabs Form 1+
AnyCubic Photon, Shining 3D EinScan-S & Atlas 3D scanners...
...and too much time on my hands.