1

Topic: Bed center problem

I need some help on a bed center problem with a model. I am trying to print a model from Thingiverse and it will not recognize the center of the bed. It keeps trying to print off the front left corner. I have tried using Netfab to fix it and Meshmixer as neither of them help. I have tried printing this using the XTZ software and also using Slic3r using settings that work with other models.

I am not familiar with gcode so I am not sure where to start with trying to figure out what the problem is. Any advice from others on how to fix this? The model is: https://www.thingiverse.com/thing:758630/#instructions

Thanks!
Ryan

2

Re: Bed center problem

The pivot point of the model is not in the center of the model. You can fix this in a modeling program.

3

Re: Bed center problem

How am I able to change the pivot point? I have tried in Meshmixer and 123Desgin, but no luck. Do I need to use a different program? Or can I change the z-offset in slic3r for this model to something like -100?

Thanks!

4

Re: Bed center problem

rcskpeters wrote:

How am I able to change the pivot point? I have tried in Meshmixer and 123Desgin, but no luck. Do I need to use a different program? Or can I change the z-offset in slic3r for this model to something like -100?

Thanks!

The z offset controls the height that the extruder starts at. If you want to center the model you would need to change the x and or y offset in slicer.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.